000 00879 a2200253 4500
005 20250517171208.0
264 0 _c20180730
008 201807s 0 0 eng d
022 _a1944-8252
024 7 _a10.1021/acsami.7b08198
_2doi
040 _aNLM
_beng
_cNLM
100 1 _aLiu, Haodong
245 0 0 _aSuppressing Lithium Dendrite Growth with a Single-Component Coating.
_h[electronic resource]
260 _bACS applied materials & interfaces
_cSep 2017
300 _a30635-30642 p.
_bdigital
500 _aPublication Type: Journal Article
700 1 _aZhou, Hongyao
700 1 _aLee, Byoung-Sun
700 1 _aXing, Xing
700 1 _aGonzalez, Matthew
700 1 _aLiu, Ping
773 0 _tACS applied materials & interfaces
_gvol. 9
_gno. 36
_gp. 30635-30642
856 4 0 _uhttps://doi.org/10.1021/acsami.7b08198
_zAvailable from publisher's website