000 | 01703 a2200481 4500 | ||
---|---|---|---|
005 | 20250516143906.0 | ||
264 | 0 | _c20131022 | |
008 | 201310s 0 0 eng d | ||
022 | _a1944-8252 | ||
024 | 7 |
_a10.1021/am400135c _2doi |
|
040 |
_aNLM _beng _cNLM |
||
100 | 1 | _aZhao, Haichao | |
245 | 0 | 0 |
_aControlled protein absorption and cell adhesion on polymer-brush-grafted poly(3,4-ethylenedioxythiophene) films. _h[electronic resource] |
260 |
_bACS applied materials & interfaces _cJun 2013 |
||
300 |
_a4536-43 p. _bdigital |
||
500 | _aPublication Type: Journal Article; Research Support, Non-U.S. Gov't | ||
650 | 0 | 4 | _aAnimals |
650 | 0 | 4 |
_aBiocompatible Materials _xchemistry |
650 | 0 | 4 |
_aBiosensing Techniques _xmethods |
650 | 0 | 4 |
_aBridged Bicyclo Compounds, Heterocyclic _xchemistry |
650 | 0 | 4 |
_aBromine _xchemistry |
650 | 0 | 4 |
_aCell Adhesion _xphysiology |
650 | 0 | 4 | _aDielectric Spectroscopy |
650 | 0 | 4 |
_aEnzymes _xchemistry |
650 | 0 | 4 | _aHumans |
650 | 0 | 4 | _aMice |
650 | 0 | 4 | _aMicroscopy, Atomic Force |
650 | 0 | 4 |
_aNIH 3T3 Cells _xcytology |
650 | 0 | 4 | _aNuclear Magnetic Resonance, Biomolecular |
650 | 0 | 4 |
_aPolymers _xchemistry |
650 | 0 | 4 | _aProstheses and Implants |
650 | 0 | 4 |
_aProteins _xchemistry |
650 | 0 | 4 | _aQuartz Crystal Microbalance Techniques |
650 | 0 | 4 |
_aTrace Elements _xchemistry |
700 | 1 | _aZhu, Bo | |
700 | 1 | _aLuo, Shyh-Chyang | |
700 | 1 | _aLin, Hsing-An | |
700 | 1 | _aNakao, Aiko | |
700 | 1 | _aYamashita, Yoshiro | |
700 | 1 | _aYu, Hsiao-hua | |
773 | 0 |
_tACS applied materials & interfaces _gvol. 5 _gno. 11 _gp. 4536-43 |
|
856 | 4 | 0 |
_uhttps://doi.org/10.1021/am400135c _zAvailable from publisher's website |
999 |
_c22657843 _d22657843 |