000 | 01330 a2200373 4500 | ||
---|---|---|---|
005 | 20250514163008.0 | ||
264 | 0 | _c20040311 | |
008 | 200403s 0 0 eng d | ||
022 | _a0305-182X | ||
024 | 7 |
_a10.1046/j.1365-2842.2003.01059.x _2doi |
|
040 |
_aNLM _beng _cNLM |
||
100 | 1 | _aKeyf, F | |
245 | 0 | 0 |
_aThe effects of HEMA-monomer and air atmosphere treatment of glass fibre on the transverse strength of a provisional fixed partial denture resin. _h[electronic resource] |
260 |
_bJournal of oral rehabilitation _cNov 2003 |
||
300 |
_a1142-8 p. _bdigital |
||
500 | _aPublication Type: Journal Article | ||
650 | 0 | 4 |
_aAcrylic Resins _xchemistry |
650 | 0 | 4 | _aAir |
650 | 0 | 4 | _aDental Restoration Failure |
650 | 0 | 4 |
_aDental Stress Analysis _xmethods |
650 | 0 | 4 | _aDenture, Partial, Fixed |
650 | 0 | 4 | _aElasticity |
650 | 0 | 4 |
_aGlass _xchemistry |
650 | 0 | 4 | _aHumans |
650 | 0 | 4 |
_aMaterials Testing _xmethods |
650 | 0 | 4 |
_aMethacrylates _xchemistry |
650 | 0 | 4 | _aMicroscopy, Electron, Scanning |
650 | 0 | 4 | _aStress, Mechanical |
650 | 0 | 4 | _aSurface Properties |
700 | 1 | _aUzun, G | |
700 | 1 | _aMutlu, M | |
773 | 0 |
_tJournal of oral rehabilitation _gvol. 30 _gno. 11 _gp. 1142-8 |
|
856 | 4 | 0 |
_uhttps://doi.org/10.1046/j.1365-2842.2003.01059.x _zAvailable from publisher's website |
999 |
_c14376601 _d14376601 |