100 1 _aDharmastiti, R
245 0 0 _aThe wear of oriented UHMWPE under isotropically rough and scratched counterface test conditions.
_h[electronic resource]
260 _bBio-medical materials and engineering
_c2001
300 _a241-56 p.
_bdigital
500 _aPublication Type: Comparative Study; Journal Article
650 0 4 _aBiocompatible Materials
_xchemistry
650 0 4 _aBiomechanical Phenomena
650 0 4 _aHumans
650 0 4 _aIn Vitro Techniques
650 0 4 _aJoint Prosthesis
650 0 4 _aMaterials Testing
_xinstrumentation
650 0 4 _aMicroscopy, Electron, Scanning
650 0 4 _aMolecular Weight
650 0 4 _aPolyethylenes
_xchemistry
650 0 4 _aProsthesis Failure
650 0 4 _aSurface Properties
650 0 4 _aTensile Strength
700 1 _aBarton, D C
700 1 _aFisher, J
700 1 _aEdidin, A
700 1 _aKurtz, S
773 0 _tBio-medical materials and engineering
_gvol. 11
_gno. 3
_gp. 241-56
999 _c11486919
_d11486919