Thermal-induced residual stresses affect the fractographic patterns of zirconia-veneer dental prostheses.
Belli, Renan
Thermal-induced residual stresses affect the fractographic patterns of zirconia-veneer dental prostheses. [electronic resource] - Journal of the mechanical behavior of biomedical materials May 2013 - 167-77 p. digital
Publication Type: Journal Article; Research Support, Non-U.S. Gov't
1878-0180
10.1016/j.jmbbm.2012.10.022 doi
Biocompatible Materials--chemistry
Crowns
Dental Veneers
Equipment Failure Analysis
Hardness
Hot Temperature
Materials Testing
Prosthesis Design
Stress, Mechanical
Surface Properties
Zirconium--analysis
Thermal-induced residual stresses affect the fractographic patterns of zirconia-veneer dental prostheses. [electronic resource] - Journal of the mechanical behavior of biomedical materials May 2013 - 167-77 p. digital
Publication Type: Journal Article; Research Support, Non-U.S. Gov't
1878-0180
10.1016/j.jmbbm.2012.10.022 doi
Biocompatible Materials--chemistry
Crowns
Dental Veneers
Equipment Failure Analysis
Hardness
Hot Temperature
Materials Testing
Prosthesis Design
Stress, Mechanical
Surface Properties
Zirconium--analysis